Differential Corrosion Behavior of High-Aluminum 304 Stainless Steel in Molten Nitrate Salts: The Roles of Rolling and Heat Treatment — Europe PMC PMID:41095338

Source
Europe PMC (en)
Original
https://europepmc.org/article/MED/41095338
DOI
10.3390/ma18194513
License (as archived)
solo-consultazione
Archived
2026-11-09T17:12:38.027Z
SHA-256 of the archived text
6d12a551cc4dbd7d1f6ce384c1136e1385dfacd003e465a875573010d8a5077d
Stable URL of this page
https://metraipolis.com/documento/dc_fd0a615beb93

How to cite

Differential Corrosion Behavior of High-Aluminum 304 Stainless Steel in Molten Nitrate Salts: The Roles of Rolling and Heat Treatment — Europe PMC PMID:41095338 — Europe PMC (en), https://europepmc.org/article/MED/41095338 (solo-consultazione); archived copy: https://metraipolis.com/documento/dc_fd0a615beb93 (Metraipolis archive dc_fd0a615beb93, sha256 6d12a551cc4dbd7d1f6ce384c1136e1385dfacd003e465a875573010d8a5077d)
BibTeX
@misc{dcfd0a615beb93,
  title = {Differential Corrosion Behavior of High-Aluminum 304 Stainless Steel in Molten Nitrate Salts: The Roles of Rolling and Heat Treatment — Europe PMC PMID:41095338},
  howpublished = {Europe PMC (en)},
  url = {https://europepmc.org/article/MED/41095338},
  note = {License solo-consultazione; archived copy https://metraipolis.com/documento/dc_fd0a615beb93; sha256 6d12a551cc4dbd7d1f6ce384c1136e1385dfacd003e465a875573010d8a5077d},
  year = {2026}
}

Archived text

The text is not reproduced here: the archive holds it as solo-consultazione (consultation only, no republication). Read it at the original source: https://europepmc.org/article/MED/41095338. Agents can read the archived copy with the MCP tool read_document.