Effects of Artificial Hydrothermal Aging on Crush Boxes Made from Glass, Carbon and Aramid Fiber-Reinforced Hybrid Composites — Europe PMC PMID:41599544
- Source
- Europe PMC (en)
- Original
- https://europepmc.org/article/MED/41599544
- DOI
- 10.3390/polym18020249
- License (as archived)
- solo-consultazione
- Archived
- 2026-11-06T18:17:20.996Z
- SHA-256 of the archived text
6b8aaff5d60a26659569093944cfa660f4e8bc9d4ff8ba0b6a0552d2dad504e2- Stable URL of this page
https://metraipolis.com/documento/dc_fa6cc78e615a
How to cite
Effects of Artificial Hydrothermal Aging on Crush Boxes Made from Glass, Carbon and Aramid Fiber-Reinforced Hybrid Composites — Europe PMC PMID:41599544 — Europe PMC (en), https://europepmc.org/article/MED/41599544 (solo-consultazione); archived copy: https://metraipolis.com/documento/dc_fa6cc78e615a (Metraipolis archive dc_fa6cc78e615a, sha256 6b8aaff5d60a26659569093944cfa660f4e8bc9d4ff8ba0b6a0552d2dad504e2)
BibTeX
@misc{dcfa6cc78e615a,
title = {Effects of Artificial Hydrothermal Aging on Crush Boxes Made from Glass, Carbon and Aramid Fiber-Reinforced Hybrid Composites — Europe PMC PMID:41599544},
howpublished = {Europe PMC (en)},
url = {https://europepmc.org/article/MED/41599544},
note = {License solo-consultazione; archived copy https://metraipolis.com/documento/dc_fa6cc78e615a; sha256 6b8aaff5d60a26659569093944cfa660f4e8bc9d4ff8ba0b6a0552d2dad504e2},
year = {2026}
}Archived text
The text is not reproduced here: the archive holds it as solo-consultazione (consultation only, no republication). Read it at the original source: https://europepmc.org/article/MED/41599544. Agents can read the archived copy with the MCP tool read_document.