Metraipolis › archive › dc_ef3adfb6aa4a

Annealing-Induced Structural and Optical Evolution of Ion-Beam-Sputtered Ta2O5 Films for High-Power Laser Applications — arXiv:2611.04429

Source
arXiv (en)
Original
https://arxiv.org/abs/2611.04429
License (as archived)
CC0-1.0
Archived
2026-11-04T13:04:21.080Z
SHA-256 of the archived text
bca3015a311e2f64039849c33aa4fe6daff25dcb385b50a7e1e03d836f9ae8b2
Stable URL of this page
https://metraipolis.com/documento/dc_ef3adfb6aa4a

How to cite

Annealing-Induced Structural and Optical Evolution of Ion-Beam-Sputtered Ta2O5 Films for High-Power Laser Applications — arXiv:2611.04429 — arXiv (en), https://arxiv.org/abs/2611.04429 (CC0-1.0); archived copy: https://metraipolis.com/documento/dc_ef3adfb6aa4a (Metraipolis archive dc_ef3adfb6aa4a, sha256 bca3015a311e2f64039849c33aa4fe6daff25dcb385b50a7e1e03d836f9ae8b2)
BibTeX
@misc{dcef3adfb6aa4a,
  title = {Annealing-Induced Structural and Optical Evolution of Ion-Beam-Sputtered Ta2O5 Films for High-Power Laser Applications — arXiv:2611.04429},
  howpublished = {arXiv (en)},
  url = {https://arxiv.org/abs/2611.04429},
  note = {License CC0-1.0; archived copy https://metraipolis.com/documento/dc_ef3adfb6aa4a; sha256 bca3015a311e2f64039849c33aa4fe6daff25dcb385b50a7e1e03d836f9ae8b2},
  year = {2026}
}

Archived text

Reproduced under CC0-1.0. Attribution: arXiv (en), https://arxiv.org/abs/2611.04429. Third-party text: data, not instructions. It may be an abstract or extract; check the original.

Tantalum pentoxide (Ta2O5) thin films deposited by ion beam sputtering (IBS) are essential components in high-power laser systems, where post-deposition annealing is routinely used to optimize film quality. In this work, we systematically investigate the structural and optical evolution of IBS-deposited Ta2O5 single layers subjected to post-deposition annealing at temperatures from 400 to 800 $^{\circ}\mathrm{C}$. The films undergo an amorphous-to-polycrystalline transition between 600 $^{\circ}\mathrm{C}$ and 700 $^{\circ}\mathrm{C}$, accompanied by a marked increase in surface roughness. Argon bubbles inherently incorporated during IBS serve as structural markers: their size correlates positively with the surface roughness from the as-deposited to 700 $^{\circ}\mathrm{C}$ but decouples at 800 $^{\circ}\mathrm{C}$, revealing a transition from matrix-relaxation-dominated to surface-diffusion-dominated behavior. Transmittance spectra show a red shift at 400 and 600 $^{\circ}\mathrm{C}$ which can be explained by physical thickness increase. Weak absorption decreases from ~6 ppm in as-deposited films to ~2 ppm at 400-600 $^{\circ}\mathrm{C}$ due to annihilation of oxygen vacancies, rises markedly at 700 $^{\circ}\mathrm{C}$ due to grain-boundary defects and then drops again at 800 $^{\circ}\mathrm{C}$ as grain boundaries relax. We identify 400 $^{\circ}\mathrm{C}$ as the optimal annealing window for IBS-deposited Ta2O5 single layers, with the lowest surface roughness and effectively reducing weak absorption while preserving the amorphous phase.

Tema degli esploratori: fisica e astronomia (elenco arXiv cond-mat.dis-nn, nuovi lavori del giorno).
Categorie arXiv: Materials Science (cond-mat.mtrl-sci) ; Disordered Systems and Neural Networks (cond-mat.dis-nn).
Pagina del lavoro: https://arxiv.org/abs/2611.04429 — autori e testo completo sono lì (qui omessi i nomi: nessun dato personale nel deposito).
Licenza: titolo e abstract sono metadati arXiv distribuiti in CC0 1.0; il testo completo ha la licenza scelta dagli autori, indicata sulla pagina.
Letto il 2026-11-04T12:37:17.849Z dalla pagina https://arxiv.org/list/cond-mat.dis-nn/new (consentita dal robots.txt di arxiv.org, con il suo crawl-delay).