Wear Performance of a Physical Vapour Deposition-Coated, Spark Plasma Sintered TiB2/Ti Composite Lubricated with Externally Introduced hBN at Temperatures up… — Europe PMC PMID:41374118
- Source
- Europe PMC (en)
- Original
- https://europepmc.org/article/MED/41374118
- DOI
- 10.3390/ma18235274
- License (as archived)
- solo-consultazione
- Archived
- 2026-11-08T08:41:04.943Z
- SHA-256 of the archived text
29dcd885e0d5e32c184c8f79073e7cb7ac0d03a94a892bfd0e86fdd759a6841b- Stable URL of this page
https://metraipolis.com/documento/dc_b4ef4b7852df
How to cite
Wear Performance of a Physical Vapour Deposition-Coated, Spark Plasma Sintered TiB2/Ti Composite Lubricated with Externally Introduced hBN at Temperatures up… — Europe PMC PMID:41374118 — Europe PMC (en), https://europepmc.org/article/MED/41374118 (solo-consultazione); archived copy: https://metraipolis.com/documento/dc_b4ef4b7852df (Metraipolis archive dc_b4ef4b7852df, sha256 29dcd885e0d5e32c184c8f79073e7cb7ac0d03a94a892bfd0e86fdd759a6841b)
BibTeX
@misc{dcb4ef4b7852df,
title = {Wear Performance of a Physical Vapour Deposition-Coated, Spark Plasma Sintered TiB2/Ti Composite Lubricated with Externally Introduced hBN at Temperatures up… — Europe PMC PMID:41374118},
howpublished = {Europe PMC (en)},
url = {https://europepmc.org/article/MED/41374118},
note = {License solo-consultazione; archived copy https://metraipolis.com/documento/dc_b4ef4b7852df; sha256 29dcd885e0d5e32c184c8f79073e7cb7ac0d03a94a892bfd0e86fdd759a6841b},
year = {2026}
}Archived text
The text is not reproduced here: the archive holds it as solo-consultazione (consultation only, no republication). Read it at the original source: https://europepmc.org/article/MED/41374118. Agents can read the archived copy with the MCP tool read_document.