Mechanistic origin of high-cycle fatigue enhancement by grain refinement in AZ81 magnesium alloy for sports equipment — Europe PMC PMID:42241416
- Source
- Europe PMC (en)
- Original
- https://europepmc.org/article/MED/42241416
- DOI
- 10.1371/journal.pone.0350435
- License (as archived)
- solo-consultazione
- Archived
- 2026-10-31T17:57:09.791Z
- SHA-256 of the archived text
297e922309acc0d681e31cc79e2b0cf29ce605a5cbf7f24d23a854ca8e7a4bb3- Stable URL of this page
https://metraipolis.com/documento/dc_679dba064b0e
How to cite
Mechanistic origin of high-cycle fatigue enhancement by grain refinement in AZ81 magnesium alloy for sports equipment — Europe PMC PMID:42241416 — Europe PMC (en), https://europepmc.org/article/MED/42241416 (solo-consultazione); archived copy: https://metraipolis.com/documento/dc_679dba064b0e (Metraipolis archive dc_679dba064b0e, sha256 297e922309acc0d681e31cc79e2b0cf29ce605a5cbf7f24d23a854ca8e7a4bb3)
BibTeX
@misc{dc679dba064b0e,
title = {Mechanistic origin of high-cycle fatigue enhancement by grain refinement in AZ81 magnesium alloy for sports equipment — Europe PMC PMID:42241416},
howpublished = {Europe PMC (en)},
url = {https://europepmc.org/article/MED/42241416},
note = {License solo-consultazione; archived copy https://metraipolis.com/documento/dc_679dba064b0e; sha256 297e922309acc0d681e31cc79e2b0cf29ce605a5cbf7f24d23a854ca8e7a4bb3},
year = {2026}
}Archived text
The text is not reproduced here: the archive holds it as solo-consultazione (consultation only, no republication). Read it at the original source: https://europepmc.org/article/MED/42241416. Agents can read the archived copy with the MCP tool read_document.